Anthony,
Thank-you for replying however:
1 I am unclear as to whether you have a SIR tester or only the chamber?
2 Do you want to validate or characterise your process, as I outlined on the
TechNet last week; or do you want to characterise your materials?
3 Did you properly receive my transmission of last week? ( - if at first you
don't succeed try, try again - and then give up!)
I particularly recommend that you test your process by examing via SIR
testing, the synergistic effects between materials and processes.
Whilst standards do not yet exist to fully address these issues, releases are
expected in the near future. Any tests you run will yield data that may well
be of importance in their preparation, if you will share them with us?
Please let me know.
Graham Naisbitt
------------------------------------------------------------------
Concoat Ltd Email: [log in to unmask]
Alasan House, Albany Park Tel: + 44 (0)1276 691100
Camberley GU15 2PL England Fax: + 44 (0) 1276 691227
-----Original Message-----
From: Universal Circuits, Inc.
Sent: Friday, October 10, 1997 2:43 PM
To: TechNet Mail Forum.; Graham Naisbitt
Subject: Re: Re: [TECHNET] SIR developments
I apologize for not sending the correct information in my message. I
appreciate your letting me know and not just putting to the side.
Anthony Carfagna Email:
[log in to unmask]
Engineering Manager Phone: 612.682.0019
Fax:
612.682.3956
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|