Looking at similar slash sheets, when the "As Received" specification value
was not listed, it wasn't required to test for it to meet the specification.
Only the stress conditions listed. You may want to for process control
purposes, and in that case, I would use the same value as after thermal
stress.
P.S. Don't forget that Mil-S-13949H has been slated inactive for new designs.
Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.
"M.Tezuka" <[log in to unmask]> Wrote:
|
| Does anybody know about MIL-S-13949/40 about "Low and very
| low profile foil
| peel strength value minimum pound per inch of width"?
|
| The table shows only after thermal stress, at elevated
| temperature and
| after
| exposure.
| Can anybody tell me what is minimum peel strength
| requirement at room
| temperature ? Where I can find ?
|
| M.Tezuka
|
| ##########################################################
| ####
| TechNet Mail List provided as a free service by IPC using
| LISTSERV 1.8c
| ##########################################################
| ####
| To subscribe/unsubscribe, send a message to
| [log in to unmask] with following text in the body:
| To subscribe: SUBSCRIBE TECHNET <your full name>
| To unsubscribe: SIGNOFF TECHNET
| ##########################################################
| ####
| Please visit IPC web site
| (http://www.ipc.org/html/forum.htm) for additional
| information.
| For the technical support contact Dmitriy Sklyar at
| [log in to unmask] or 847-509-9700 ext.311
| ##########################################################
| ####
|
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|