I have seen a very interesting report done by Irlandus circuits IRELAND
It was done with Coates LPISM using 4 different finishes and a few
different fluxes. They have some interesting graphs that show the
relationship between different fluxes and LPISM
You can get a copy of the report from Irlandus or ASI/ Coates
AFRI Canada
On Mon, 29 Sep 1997, Phil Bavaro wrote:
> We have run some preliminary experiments with this soldermask after running
> the same testing on about six other mask materials.
>
> The results were good enough to convince us to try some real production
> lots with it. We are right in the middle of this confirmation effort at
> present.
>
> Solderball free was not an accurate description, but the preliminary
> results indicated a 90% reduction compared to next best mask.
>
> We currently use Enthone DSR-3241 which leaves plenty of wavesolderballs
> (although they are very small) behind.
>
> As far as the comment about the relationship between the mask and the
> wavesolderballs, it is only one factor in a complex process, however it is
> a factor which we can control. Quantity of flux applied to the board and
> the preheating have to also be optimized for the least conducive conditions
> to create solderballs.
>
> I would appreciate hearing any information/comments on this subject as this
> has been a thorn in our sides for a long time now.
>
>
> Phil
> ------
>
>
>
> At 2:40 PM +0300 9/29/97, Johannes Sivula wrote:
> >Hi,
> >You wrote:
> >
> > Could anyone share any experiences with me about Carapace Electra LPI
> > which was claimed solder ball free with no-clean?
> > Please reply to me directly.
> > As always, look forward to your helpful replies.
> > Thanks,
> > Yuan
> > Exabyte
> >
> >
> >
> >Did you get any replies ? If you get any, please forward them to me.
> >I would appreciate that.
> >By the way, how did you come by the idea that solder balling has something
> >to do with solder mask ?
> >I have read that that is the case, but I have not seen any serious report
> >to back up my idea.
> >Brs,
> >Johannes Sivula, Reliability Engineer,
> >Tellabs Oy
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> >following text in the body:
> >To subscribe: SUBSCRIBE TECHNET <your full name>
> >To unsubscribe: SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> >additional information.
> >For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> >847-509-9700 ext.311
> >##############################################################
>
>
>
> Phillip A. Bavaro
> Senior Manufacturing Engineer
> [log in to unmask]
> (619) 658-2542
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|