TECHNET Archives

October 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Date:
Thu, 9 Oct 1997 15:26:15 +0900
Content-type:
text/plain; charset=euc-kr
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (83 lines)
Need more information such as technical brochure on your Palladium System.


    Jin-Ho Lee,      R & D Director

    Daeduck Electronics Co
     390-1 Mognaedong , Ansan city
     Kyungkido   425-100
     KOREA

     [log in to unmask]






[log in to unmask] on 97-10-08 01:59:16 ¿À

±îÁö [log in to unmask]¿¡°Ô ȸ1/2ÅÇÏ¿(c) ÁÖ1/2Ê1/2ÿÀ.; ±îÁö [log in to unmask]¿¡°Ô ȸ1/2ÅÇÏ¿(c) ÁÖ1/2Ê1/2ÿÀ.


TO:      [log in to unmask]
CC:       (ºñ¹ÐÂüÁ¶ÀÎ: ÀÌÁøÈ£/DAEDUCK)
SUBJECT: Re: [TECHNET] Palladium



Content-type: text/plain; charset=us-ascii


One of the lesser known, most unique, least expensive, and trouble free
Palladium plating systems is offered by RD Chemical Company.  It is called
the Paladin(TM) system, and it is the  only IMMERSION Palladium plating
system available commercially, as compared to the other ELECTROLESS
Palladium
plating systems.
Immersion plating systems (versus electroless) are much easier to run, much
less prone to give you spurious, or unwanted plating, much less expensive,
and are self limiting.  The deposits tend to be less porous, and smoother
than electroless, because they are metal exchange plating systems, and will
plate only on to a specific substrate, in this case Copper, and when all
the
Copper is covered, plating ceases.
The bath is a fabricators dream come true, because it is possible to put a
lid on the bath for a year, come back, heat it up, and it will plate like
it
did a year ago.  There are only two controls, pH, and metal content.  And
further, it does not build Copper in the bath, as when the Copper builds to
150 ppm, it starts falling out, and is simply filtered out.
Apologies to those offended by any potentially commercial aspects that they
believe they see in this message.  Further information cheerfully available
off line.
Rudy Sedlak
RD Chemical Company
Phone (650) 962-8804
fax (650) 962-0370
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2