======== Original Message ========
Hi Technters.
Looking for a way to verify my panels were baked at the correct
temperature. I would like to find a way of incorporating a system into
production without too much fuss.
Omega sells heat sensitive markers the range I am looking for.
Does anybody have experience with these markers? Do they come off
easily? Do they contaminate some chemistries while being processed? Or
any other reservations?
I have also seen microdot labels but I am reluctant to use those
since it involves placing and removing them before processing. Is there
something else out there that would work?
Thank you
[log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
======== Fwd by: Richard MacCu ========
Install a data logger on your oven. It should accurately track the time and
temperature of the oven. Then by using an oven log for baked panels you
have a hardcopy of the day's baking parameters.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################