During 1989 and 90 we used to get our HAL Bath Solder analysed from

                        GSI Spectroscopy
                        2227 Martinique Lane
                        Oxnard, Ca 93035  Fx: 805/785-7286

There service used to be very prompt and even sitting in India we used
to get the results by fax within a week. We lost track of them since
then, the company has probably merged with some other entity. Does
anyone know of its whereabouts or its fresh coordinates? Any suggestions
for similar service provider who is quick and cost effective. In those
days they used to charge US$55 per sample.
PV Khan
Chief Quality Manager
Linaks Microelectronics Limited
Lucknow, India
Fax:+91-522-315953, 222061
email: [log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2