[log in to unmask] wrote:
>
> Techneters:
> I have recently experienced a hole wall pullaway issues on various
> product. I completed a DOE using various dep chemistries and various
> plating chemistries. The results were inconclusive. Is anyone aware of
> a root cause for hole wall pullaway unrelated to the Electroless
> process.
>
> Thanks in advance for any input
Does the process have black oxide or double treat? How much nailheading
do you see?
Drilbert