Techneters:
I have recently experienced a hole wall pullaway issues on various
product. I completed a DOE using various dep chemistries and various
plating chemistries. The results were inconclusive. Is anyone aware of
a root cause for hole wall pullaway unrelated to the Electroless
process.
Thanks in advance for any input