TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
SMTPGATE <[log in to unmask]>
Date:
Thu, 4 Sep 1997 09:18:58 -0400
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, SMTPGATE <[log in to unmask]>
Parts/Attachments:
text/plain (17 lines)
Mail*Link¨ SMTP               [TECHNET] FAB: Acceptabilty of dents

Fellow Tech-Netters:

Some of the high-volume single-sided boards we produce are punched. At times
we find repetitive dents on the surface of each board where a laminate chip
has lodged on the face of the die, causing a slight depression with each hit
until it is cleared away. These dents are typically no more than .050" in
diameter and do not cut foil or reduce cross section, just depress it a bit
into the base laminate (1/0 .062" CEM-1 or FR-4). Is anyone aware of an IPC
spec or other reason why these class 1 and 2 boards should be rejected?
In the absence of these, personal opinions on acceptability would also be
appreciated.

Bill Parlin