>Subject: [TECHNET] ASSY: BENCH (HAND) CLEANING SURVEY
>
>I'm doing a survey to determine how others in industry are cleaning (assuming
>you do clean) flux residue from hand soldering operations like soldering
>wires
>to terminals on small sub-assemblies, etc. I'm really interested in military
>hardware, but all can reply. My questions are as follows:
>
>1) Military or Commercial?
> 90% Mil 10% Other
>2) Clean or no clean?
> Clean
>3) What flux type are you using?
> RMA
>4) Hand or machine cleaning?
> 98% in-line / 2% hand
>5) What chemical or solvent are you using?
> Axarel 32 / IPA
>6) Are you happy with your present cleaning process?
> Yes, in-line cleans very well.
>7) Any additional comments?
>
>Thanks for your time and cooperation. I will tabulate all of the results and
>post it on Technet when complete.
>
>Jim Marsico
>(516) 595-5879
>[log in to unmask]
>
> ********************************
> * ______ _ _ _____ *
> * / ___ | | | | | _____ *
> * / /___| | | | | | _____ *
> * __/ ____ | | | | |______ *
> * |____/ |_| |_| |________| *
> * *
> * SYSTEMS, INC. *
> ********************************
>
|
|
|