TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Robinson, Mike (AZ75)" <[log in to unmask]>
Reply To:
TechNet Mail Forum.
Date:
Wed, 20 Aug 1997 15:59:53 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (20 lines)
Marti,

If the pad is the same width as the lead, you can't form side fillets. Per
the PWB Design guidelines we have a minimum of 1.5 mils on each side on our
20 mil pitch and even more at larger pitches. There's and equation used for
each lead with and type.

Since 45 degree screening is not an option, consider squeegee pressure,
speed, and material for optimum solder on axis usually low on volume. Are
using fine pitch paste which has smaller particles than regular SMT paste.

Mike Robinson
 ----------