Greetings:

I have a question regarding moisture in LN2 Dewars.  My assumption is under
normal conditions, the moisture would be frozen solid and have a very low
vapor pressure, but what happens to the ice as the dewar becomes empty...
anyone else experienced a problem that could be attributed to moisture in a
LN2 system?