Hi Duane,
It is not an oxide treatment, but you might try the Gould people, who can
supply the standard copper treatment that they supply on their copper foil. My
contact there in the past has been Rolly Savage.
Good Luck,
Les Connally
[log in to unmask]
> From: "Duane B. Mahnke" <[log in to unmask]>, on 7/30/97 9:04
> PM:
> Dear Technetters,
>
> I am looking for vendors who could treat 10 mil thick copper with an
> oxide treatment for bond enhancement. Please answer me directly with
> information, as I don't want this to turn into an ad campaign on the
> technet. Names and addresses can be faxed to my attention at
> 602-917-5256 or by direct E-Mail at [log in to unmask]
>
> Your help would be most appreciated.
>
> Duane Mahnke
>
> Remember - Just do it!!! Planning is a form of procrastination!!!
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
>
|
|
|