     People:

     Does anyone have maximum pull strength figures (in pounds) for a
     straight inserted lead into an 0.062 thick PCB. The leads are 0.040"
     to 0.080" diameter, and the PTHs are 0.007" to 0.010" larger than the
     leads.  The solder is 63/37.  Both the lead and the PTH are solder
     plated over copper.