TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
X-To:
Date:
Fri, 8 Aug 1997 11:13:31 -0700
Reply-To:
Subject:
From:
Butch White <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
Organization:
CEMCO
MIME-Version:
1.0
Parts/Attachments:
text/plain (23 lines)
[log in to unmask] wrote:
>
> Hey Russ -
> You are not alone - most of the HASL systems out there do not appear capable
> of providing adequate coplanarity for microBGA and very fine-pitch.  Gold
> flash of course will work fine.  Of course there is the phobia of gold
> embrittlement and whether this is a problem or not will depend upon the
> application and the reliability (life) aspects of it.  I've had very good
> luck with OSPs and CSP and recommend you seriously consider that route.
> Best regards,
> Phil Zarrow
> ITM, Inc.
> Durham, NH
> (ps: see you at SMI !?!)

Gents,  CEMCO will be happy to run evaluation testing on our horizontal
system at our UK factory or at our service in Scotland.
--