Hi L Connally
Can you confirm that the use of iodine (even at 1PPM) will have no effect on product contamination.
Regards
Andy McKean
[log in to unmask]
-----Original Message-----
From: mailnet
Sent: Thursday, August 14, 1997 9:21 AM
To: Andy R.J. McKean
Subject: "Leslie O. Connally" <[log in to unmask]>: re: [TECHNET] Micro-organisms in rinses
From: "Leslie O. Connally" <[log in to unmask]>
Hi A. McKean,
I'm not sure as to how to measure it, but about 1 PPM of Iodine in the
water will kill most of the Microorganisms. We used this to kill algae in DI
Water.
Regards,
Les Connally
[log in to unmask]
> From: Andy RJ McKean <[log in to unmask]>, on 8/14/97 9:05 AM:
> Looking for info. on the effects and measurables of micro-organism growth in
> rinse water. We have had a supplier mention this as a new problem occuring
> in Europe.
>
> A. McKean
>
>