I don't know of anyone making graphite reinforced laminate for the
circuitboard industry. It is used in structural and military and athletic
fields. You could try one of the military fabricators. Don't forget, however.
that carbon is a conductor!
J S Sallo
Sallo Consulting Services
760 346 6717