TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
"D. Rooke" <[log in to unmask]>
Date:
Mon, 18 Aug 1997 19:08:57 -0400
Content-Type:
text/plain; charset="us-ascii"
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, "D. Rooke" <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
We have been using RT foil for almost 2 years here at Circo Craft and have
not found any significant degredation in performance for standard FR4 with
conventional oxide. Both reverse treat and conventional foil substrates have
successfully passed numerous reliability assessments including 1000 hour
air-to-air thermocycling, liquid-to-liquid thermocycling, IST and T260
delamination test. As far as reliability is concerned we have found no
difference (not better; not worse).

What would make you think that the RT (ie DSTF) foil would be MORE reliable??

Dave Rooke
Circo Craft - Pointe Claire
a division of Viasystems

= = = = = =

>Hi to All,
>
>I have a question. Do you think that inner layers produced on base material
(FR4) with drum side treated copper foil is more reliable than inner layers
produced on standard base material followed by black or brown oxide?
>
>Thanks for your time.
>Cristian
>
>