TECHNET Archives

August 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Robert Schetty <[log in to unmask]>
Date:
Thu, 14 Aug 1997 18:32:27 UT
X-cc:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Robert Schetty <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
        The data that I've seen on this subject indicates that very smooth Ni/Au
surfaces wire bond poorly.  On the other hand, an extremely rough Ni/Au
surface also exhibits poor wire bond pull strengths.  In general, it seems a
"moderately rough" Ni/Au surface provides the best results.

Rob Schetty
LeaRonal Inc.


----------
------------------------------------------------------------------------------
-------------------------
A question came up on what the surface finish (smoothness/roughness) should
be for wire bond on a land.  The plated finsh is typically nickel and a
covered with a soft gold finsh.  Will hills and valleys in the surface make
any difference in the bond strength.

Phil Hinton
hintpwb1@aol,com