Richard,
I've heard once about such thermal labels but I don't think they will be able to tell you the whole story about what the board went through inside the reflow.
A company named "Electronic Controls Design Inc." has a product - "M.O.L.E".
This is a recorder that can be passed through the reflow oven and then connected to a PC (equipped with the matching software). Then you can get the exact temperature profile the recorder went through.
I think this can give you easy and accurate measurements of the temperature profile inside your reflow oven.
The companie's full name and address:
---------------------------------------------------------
Electronic Controls Design Inc.
4287A SE International Way
Milwaukie, OR 97222-8825 U.S.A
(800) 323-4548 Outside Oregon
(503) 659-6100 Within Oregon
FAX (503) 659-4422
---------------------------------------------------------
If you want further details, contact me directly through my E-mail and I'll be glad to provide all the information I can get for you.
Yehuda
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|