recently paul said that if you are using  alkaline etching your can not
produce fineline ( < 6 mil).almost all alkaline etching solution suppliers
claim that  their replenisher is formulated for fine lines and can be used
for etching inner layers ( print & etch ) using dryfilm as etch resist. Even
all recycling etch manufactuerers claim that their ammonical recycling
etching systems are being used for producing fineline innerlayers. any
feedback / discussion will be appreciated.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2