Mike 

Standard for the industry is 6 and 6 for line width and space most shops
can do 5 and 5 without a problem but 6 and 6 is standard for production
houses.  Prototype vendors can do much tighter some down to 2 and 2 but
this tight has a high risk and fall out.   Your vendor choices must be made
on a cost vs reliability need choice.

Good Luck!

Jon Johnson
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2