Hi Ingemar!
If you are after your time then so are a whole bunch of the rest of
us! Yes, problems with solderability and reliability of having a gold
finish over a copper and/or copper alloy base metal without a barrier
to prevent diffusion issues is still a problem reported within the
electronics industry from time to time. Sometimes it appears we have
to "re-learn" certain lessons.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: Koax plating
Author: [log in to unmask] at ccmgw1
Date: 6/12/97 8:22 AM
Question: We have bought subminiature coax connectors for SMT. They have
2um Gold over Brass (body) without Nickel barrier. I don't like the risk
of Zn-leakage. Am I too oldfashioned? People put Tin directly on Kovar
terminals etc. As I cannot handle roller blades, and has spent many
years in a Quality Lab, I may be after my time....../Ingemar /EMW
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|