Hi Tomer,
Permanganate hole preparation solutions will remove small amounts. For big
jobs concentrated sulphuric acid takes some beating.
regards,
Dave Heywood
[log in to unmask]
----------
From: [log in to unmask]
To: [log in to unmask]; Dave Heywood
Subject: Remove prepreg
Date: 16 July 1997 08:02
<<File Attachment: ENVELOPE.TXT>>
Hello everybody
I need some advise
Does somebody know how to remove resin (prepreg) from copper surface by
chemical means ??
Thanks in advance for any help
Tomer
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************