Hi Tomer,
Permanganate hole preparation solutions will remove small amounts. For big 
jobs concentrated sulphuric acid takes some beating.
regards,
Dave Heywood
[log in to unmask]
 ----------
From: [log in to unmask]
To: [log in to unmask]; Dave Heywood
Subject: Remove prepreg
Date: 16 July 1997 08:02

<<File Attachment: ENVELOPE.TXT>>
Hello everybody

I need some advise

Does somebody know how to remove resin  (prepreg) from copper surface by

chemical means ??

Thanks in advance for any help

Tomer

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2