Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset=US-ASCII |
Old-Return-Path: |
|
Date: |
Mon, 21 Jul 1997 14:44:51 -0500 |
Precedence: |
list |
Resent-From: |
|
Message-ID: |
|
From [log in to unmask] Tue Jul 22 14: |
35:31 1997 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wqO2Q-000BjfC; Mon, 21 Jul 97 14:22 CDT |
Content-Description: |
cc:Mail note part |
Subject: |
|
From: |
|
>From willli Mon Jul 21 14: |
22:45 1997 |
Resent-Message-ID: |
<"SzCRS3.0.EGB.rRxqp"@ipc> |
Content-Transfer-Encoding: |
7bit |
Resent-Sender: |
|
Parts/Attachments: |
|
|
What would be the difference with using a Dessicant package or
CopperTex? Your acheiving the same results with a different medium,
YES? Will someone explain. I to am having problems with outdated
components. I am having our warehouse identify all components with
date codes outside a 12 months reriod prior to kitting. Hence, the
kit part, we consign, so once the drypack is open, I need a quick and
efficient alternative to minimizing Tin-Lead oxidation and Moisture.
Please advise.
Thank you.
John Gulley
______________________________ Reply Separator _________________________________
Subject: Re: Oxydation arrest paper
Author: [log in to unmask] at Internet
Date: 7/21/97 1:27 PM
We use a paper Called Coppertex which can be obtained from St. Louis Paper
314-531-7900, Talk to Les Peters.
Comes in Rolls of 36" or 48".
[log in to unmask] on 07/21/97 01:47:03 PM
To: [log in to unmask]
cc: (bcc: Bob R Boilard/LABARGE)
Subject: Oxydation arrest paper
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|