TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wotiM-000BjhC; Thu, 17 Jul 97 11:47 CDT
Content-Type:
text/plain; charset=us-ascii
CC:
Old-Return-Path:
Date:
Thu, 17 Jul 1997 09:07:25 -0700
Precedence:
list
Reply-To:
Message-ID:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14084
TO:
X-Status:
Return-Path:
<TechNet-request>
X-Loop:
Resent-From:
Resent-Message-ID:
<"9hCnd.0.yBB.foapp"@ipc>
Content-Transfer-Encoding:
7bit
>From willli Thu Jul 17 11:
47:57 1997
From [log in to unmask] Mon Jul 21 15:
56:01 1997
From:
Dan Brandler <[log in to unmask]>
Subject:
X-Mailer:
Mozilla 3.0C-NSCP (Win16; U)
Organization:
Ohmega Technologies, Inc.
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (22 lines)
To: TechNet

We have a mildly acidic citrate type plating bath that develops MOLD
after periods of unuse, usually within two to three weeks. The mold
stains the deposit and plugs the filters. We prefer not to use
formaldehyde as a biocide due to its toxicity.

Can anyone recommend a benign biocide? Please advise.

Daniel Brandler, Ohmega Technologies, [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2