TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0woOkN-000BkHC; Wed, 16 Jul 97 02:43 CDT
Content-Type:
text/plain; charset=ISO-8859-1
Old-Return-Path:
Date:
Wed, 16 Jul 1997 8:32:43 +0000
MIME-version:
1.0
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Mon Jul 21 10:
21:27 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/14030
TO:
Content-transfer-encoding:
quoted-printable
>From willli Wed Jul 16 02:
43:55 1997
Status:
O
Resent-Message-ID:
<"G23Th1.0.2Z7.fk7pp"@ipc>
Subject:
From:
X-Loop:
Return-Path:
<TechNet-request>
X-Mailer:
TFS Gateway /221000000/221040953/221001499/221081163/
Message-Id:
Parts/Attachments:
text/plain (47 lines)
Hi Tomer,
Permanganate hole preparation solutions will remove small amounts. For big 
jobs concentrated sulphuric acid takes some beating.
regards,
Dave Heywood
[log in to unmask]
 ----------
From: [log in to unmask]
To: [log in to unmask]; Dave Heywood
Subject: Remove prepreg
Date: 16 July 1997 08:02

<<File Attachment: ENVELOPE.TXT>>
Hello everybody

I need some advise

Does somebody know how to remove resin  (prepreg) from copper surface by

chemical means ??

Thanks in advance for any help

Tomer

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2