TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wo9J4-000BkKC; Tue, 15 Jul 97 10:14 CDT
Encoding:
37 Text
Old-Return-Path:
Date:
Tue, 15 Jul 97 10:23:39 cst
>From willli Tue Jul 15 10:
14:51 1997
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
From [log in to unmask] Mon Jul 21 10:
11:46 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/14008
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"r3I05.0.4s7.GFvop"@ipc>
Subject:
From:
Status:
O
Precedence:
list
X-Loop:
Message-Id:
Parts/Attachments:
text/plain (49 lines)
     Hi TechNet -
     
     If there is no barrier plating finish between the silver and the brass 
     (such as nickel) then you may have zinc diffusion into/thru the silver 
     finish which will make for an nonsolderable situation. Conduct a 
     microsection and scanning electron microscopy analysis on the part to 
     determine the metallurgies present and to verify the finish 
     measurements. Good Luck.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator _________________________________
Subject: Soldering silver on brass
Author:  [log in to unmask] at ccmgw1
Date:    7/15/97 8:42 AM


     
     
     I have a part which is brass with 1 um of Ag. It does not take solder 
     very well at all. Any suggestions?
     
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2