ALZA Corporation, Minneapolis MN, is in need of a solder expert to
help to resolve a problem we are having with cracked/separated solder
joints on some of our surface mount capacitors. Can you recommend
someone, preferably in the Minneapolis area, who would consider
consulting with us on this problem? If so, please contact me at
[log in to unmask]
***************************************************************************