Many solder suppliers also offer temporary solder mask. The problems you can
expect from some of these masks are:
- Adhesion problem at high temperature
- Compatibility with the wave flux you use
- Printability issues (if screen print)
- Residue left on pads after removal
- Compatibility with your wash equipment (if water soluble)
- Cure time
- Fracture druing thermal cycle (Thickness dependent)
Internet is a very good sources to start your search.
Hope this helps,
Michael Yuen
----------
From: TechNet-request
To: TechNet
Subject: Temporary Spot Solder Mask
Date: Wednesday, July 23, 1997 11:30AM
We are currently testing and looking at a latex peelable, a water-soluble,
a UV peelable, and a UV water-soluble.
I was wondering what type of temporary spot solder mask was out there and
what type are companies using and why?
I would also like to know if there were any problem that occured with the
spot mask during the wave or cleaning process ?
Thank you,
Benjamin Lee
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|