SERA is Sequential Electrochemical Reduction Analysis. The technique can
detect and quantify the oxides and other reducible species on the metal and
alloys surfaces. The presence of the soldermask residue can be monitored on
the copper too.
Regards
Mike Pavlov
***************************************************************************