Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="iso-8859-1" |
Old-Return-Path: |
|
Date: |
Wed, 9 Jul 1997 17:54:35 -0800 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
Content-Transfer-Encoding: |
quoted-printable |
Status: |
O |
X-Mailing-List: |
|
X-Sender: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"skGoq2.0.zgB.c23np"@ipc> |
>From willli Wed Jul 9 19: |
45:43 1997 |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wm7MN-000BjfC; Wed, 9 Jul 97 19:45 CDT |
In-Reply-To: |
|
From [log in to unmask] Thu Jul 10 08: |
50:26 1997 |
Message-Id: |
<v0310280cafe9ef6050a0@[129.46.191.246]> |
Parts/Attachments: |
|
|
Almost any of the benchtop flowing solderbath systems on the market will
work. Hakko, air-vac, etc. Just look for ones which have nozzles
designed for the removal of PGA's.
We have used a Hakko system which has interchangeable nozzles for years.
It is ideal for PGA's because it centers the board over the nozzle with a
light beam and it has an analog timer which can be programmed to indicate
when to extract the component.
One word of caution......don't pull the PGA out until you are sure that all
of the connections have melted. I have seen operators pull the barrels
right out of the boards still attached to the component.
Hope this helps.
At 4:13 PM -0800 7/9/97, Tom Hybiske wrote:
>Does anyone know of a commercially available tool for de-soldering
>PGA's, specifcally 144 PGA's from assembled printed wiring boards?
>
>Thanks,
>Tom Hybiske
>General Atronics Corp.
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
>* with <subject: subscribe/unsubscribe> and no text in the body. *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
>***************************************************************************
Phillip A. Bavaro
/\ /\
\ /\ \ /\
( ) ( )
.( o ). .( o ).
==============
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|