TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wrnCj-000BkQC; Fri, 25 Jul 97 11:26 CDT
Old-Return-Path:
Date:
Fri, 25 Jul 97 10:22:22 MDT
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14311
TO:
Return-Path:
<TechNet-request>
>From willli Fri Jul 25 11:
27:22 1997
Resent-Message-ID:
<"k2iag1.0.6sF.FFDsp"@ipc>
Subject:
From:
X-Loop:
Cc:
From [log in to unmask] Mon Jul 28 09:
43:11 1997
Message-Id:
Parts/Attachments:
text/plain (61 lines)
     Thanks for the information. I have not been able to find information 
     on Dynaco, Teledyne and EMC rigid-flex on the internet. Does anyone 
     know how to contact these companies? Any paper or book to recommend?
     
     Thanks,
     
     Yuan (303)417-5655


______________________________ Reply Separator _________________________________
Subject: Re: Rigid-flex technologies
Author:  [log in to unmask] at UNIXMAIL
Date:    7/25/97 6:37 AM


There are three basic types of rigid-flex product.  The oldest 
versions use acrylic adhesive constructions to bond the copper to the 
flex layers and have always struggled with the thermal mismatch of 
the materials.  With the advent of adhesiveless laminates, the 
technology became more robust.  Both of these technologies are 
available from any of the manufacturers of rigid-flex.  These 
include, but are not limited to, Parlex, Dynaco, Teledyne, EMC, 
Strataflex, Pioneer, Multiflex and FCI.  I've tried to list them all.
     
The problem with rigid-flex has always been cost.  Functionality is 
outstanding, but the commercial world can't afford the cost.  Several 
technologies are available that are trying to make R/F practical for 
commercial applications.  Teledyne came out with the first, 
Regal-Flex and that technology is avaible through GulTech, Hadco and 
Teledyne.  Parlex then developed the PALCore process, which uses 
resin coated copper cap layers to build thin and low cost boards, and 
still holds that technology exclusively.  EMC had their own process 
also and now Hadco has announced their HVR product that is similar to 
Regal-Flex.  
     
If you contact Hadco, Parlex, Teledyne and EMC, you will have access 
to information on the key and different rigid flex technologies on 
the market.
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   * 
* with <subject: subscribe/unsubscribe> and no text in the body.          * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2