TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wrmVn-000BlJC; Fri, 25 Jul 97 10:42 CDT
Old-Return-Path:
Date:
Fri, 25 Jul 97 11:50:24 EST
Precedence:
list
Resent-From:
>From willli Fri Jul 25 10:
42:56 1997
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14307
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"Jh2ZX3.0.PZB.oaCsp"@ipc>
Subject:
From:
X-Loop:
From [log in to unmask] Mon Jul 28 09:
42:49 1997
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
Parts/Attachments:
text/plain (20 lines)
     Hello!
     Has anyone experienced Deep or Tab gold plate passing tape test at the 
     precious metal process, only to have gold peel after the Hot Air 
     Solder Level process.
     
     Thanks
     
     Carlos

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2