TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wrTYH-000BlGC; Thu, 24 Jul 97 14:27 CDT
Content-Type:
text/plain; charset=ISO-8859-1
Old-Return-Path:
Date:
Thu, 24 Jul 1997 13:35:48 -0600
Precedence:
list
From [log in to unmask] Mon Jul 28 09:
39:10 1997
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14280
X-MSMail-Priority:
Normal
X-Status:
Return-Path:
<TechNet-request>
>From willli Thu Jul 24 14:
28:16 1997
X-Loop:
Resent-From:
Content-Transfer-Encoding:
7bit
Resent-Message-ID:
<"Quw4F.0.ACD.oowrp"@ipc>
Subject:
From:
"Steve Collins" <[log in to unmask]>
TO:
"TechNet" <[log in to unmask]>
X-Priority:
3
X-Mailer:
Microsoft Internet Mail 4.70.1155
Message-Id:
Parts/Attachments:
text/plain (27 lines)
I have a .035 dia soldermask pad with no hole in a circular array pattern
that I use over our mounting holes so we can skip a spot mask process in
manufacturing. My question is : is this size pad too small to expose or
develop when using LPI soldermask . I have two vendor who are having
trouble with this pattern and when I get the boards in I have what looks
like exposed copper contained on some of the pads. We know that they are
not really exposed or else they would have covered in the HASL process or
would be discolored due to contamination. The pads are just as bright
copper color as you would expect to see before LPI soldermask is applied.
Anyone have any thoughts.

Steve Collins
PCB Design Supervisor
Antec
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2