TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Tue, 22 Jul 1997 15:27:29 +0200
Precedence:
list
Resent-From:
>From willli Tue Jul 22 08:
17:06 1997
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Tue Jul 22 14:
38:18 1997
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14190
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"auOYm3.0.r4A._ABrp"@ipc>
Subject:
From:
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wqeo4-000BkRC; Tue, 22 Jul 97 08:16 CDT
X-Mailer:
Windows Eudora Pro Version 2.2d (16)
Message-Id:
Parts/Attachments:
text/plain (33 lines)
We need polyimide flexible jumpers for nuclear detector feedthrough
fabrication. The geometric specifications are as following :
number of conductive lines : 36
pitch : 1 mm (distance between the axis of twoo adjacent lines)
width of a line : 0.5 mm
length of the flexible : 300 mm
materials : the conductive lines are inserted between 2 polyimide foils.
contacts : lines are ended by a contact on both sides for soldering.

We are interested by any similar product (but different for one or more of
our parameters) that would avoid the tooling charge.

Does anybody a company that might have such products.

Thank you very much

      _/   _/         _/                 Bruno Guerard
     _/   _/         _/                  email:[log in to unmask]
    _/   _/         _/                   Institut Laue-Langevin
   _/   _/         _/                    B.P.156, 38042 Grenoble Cedex 9, France
  _/   _/_/_/_/   _/_/_/_/       tel:(33) 76.20.72.77 fax:(33)76.20.77.00

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2