TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wpEWY-000Bk0C; Fri, 18 Jul 97 10:00 CDT
Old-Return-Path:
Date:
Fri, 18 Jul 1997 11:11:33 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/14113
>From willli Fri Jul 18 10:
01:18 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"AK2_Z2.0.oaK.WKupp"@ipc>
Subject:
From:
Message-ID:
X-Loop:
From [log in to unmask] Mon Jul 21 16:
02:14 1997
Parts/Attachments:
text/plain (26 lines)
Pink ring by itself is cosmetic - and is an indication
of a less than perfect process.

The caution is if you have pink ring YOU COULD HAVE
WEDGE VOIDS. and this is where the functional problems
come up.  

When I see obvious pink ring, then multiple microsections
should be performed to assure no wedge voids are present.
If they are not and the hole wall plating is continuous, then
the boards are not a realiability threat (for that reason).

Susan Mansilla
Robisan Lab

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2