Address,
Are there any Technical Publications on comparing the reliability of
unsupported and supported vias/pths? What other avenues should I be
concerned with should I have unsupported vias and pths (internal and
external) where conductors do not intersect?
My reading up until now says supported vias and pths are more reliable
than there counterparts. Does this still hold true? All other vias
and pths will have A/Rs and teardrop pads with no tangent and/or
breakout at the egress.
Pass the info. Please advise. Later
John Gulley
***************************************************************************