TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wnmvQ-000BkkC; Mon, 14 Jul 97 10:20 CDT
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Mon, 14 Jul 1997 11:34:25 -0400
Precedence:
list
Resent-From:
Message-ID:
MIME-Version:
1.0
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13964
From [log in to unmask] Mon Jul 14 13:
23:52 1997
>From willli Mon Jul 14 10:
20:53 1997
TO:
Return-Path:
<TechNet-request>
X-Status:
Resent-Message-ID:
<"dkYmj2.0.IKI._Eaop"@ipc>
Subject:
From:
John Nelson <[log in to unmask]>
X-Loop:
Cc:
Content-Transfer-Encoding:
quoted-printable
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (40 lines)
Thermal cure inks are what is normally used for via plugging because it is hard to 
get light into the holes to set up a uv ink and it is hard to get solvent out of holes at
bake.  The most common ink used for plugging is SR-1000.  We use green.  
In a previous life we used clear.

----------
From: 	[log in to unmask][SMTP:[log in to unmask]]
Sent: 	Monday, July 14, 1997 6:11 AM
To: 	[log in to unmask]; [log in to unmask]
Subject: 	Unidentified subject!

Is there anyone out there using thermal cure type inks for via plugging?  Are there any advantages to using these inks (as opposed to UV cureable)?

Jamie McIntyre
PCI

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************




***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2