TECHNET Archives

July 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wnmAx-000Bn9C; Mon, 14 Jul 97 09:32 CDT
Old-Return-Path:
Date:
Mon, 14 Jul 1997 09:22:45 -0400 (EDT)
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13948
From [log in to unmask] Mon Jul 14 13:
22:17 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"t8NPI.0.6uJ.-XZop"@ipc>
Subject:
From:
>From willli Mon Jul 14 09:
32:46 1997
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (35 lines)
Gents,

there has been a bunch of mails with respect to solder compatibility but to
be
honest I`m more confused than before. The initial question about mixing 63/37
tin-lead solder plating with 96.5/3.5 silver-tin wave solder process with
respect to intermetallics produced some replies - but:

1. How do I manage to get rid of nearly all of the lead by a wave soldering
pro-
    cess ? Anybody who can tell how much of the 63/37 solder is washed away ?
    While handsoldering I experienced that pretinning a 63/37 tin-lead solder
plating
    with Sn96 - even if done more than once - will not result in a plain Sn96
finish.
    You will still find amounts of lead in the range of 0.6 - 5%.

2. What is the final solder composition if lead is still a part of it and
what about the
    physical/mechanical properties ? Doesn`t 1% (or less) will decrease the
melting
    point? Couldn`t be silver washed away ? And what about the mechanical
proper-ties of 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2