We have been working with a customer for over a year and they have found the
following deposition acceptable for their customers:
elni - 100 min to 150 microinches
imau - 4 - 6 microinches
Of course total coverage of the panel surface is a must.
regards
richard fudalewski
atotech canada ltd
***************************************************************************