From [log in to unmask] Fri Jun 6 15: |
35:51 1997 |
Old-Return-Path: |
|
Date: |
Fri, 6 Jun 97 12:46:44 PDT |
Precedence: |
list |
Resent-From: |
|
>From willli Fri Jun 6 14: |
35:59 1997 |
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wa4nf-000BjGC; Fri, 6 Jun 97 14:35 CDT |
X-Priority: |
3 (Normal) |
Resent-Message-ID: |
<"4m3si.0.wmF.MQ6cp"@ipc> |
Subject: |
|
From: |
|
X-Incognito-Format: |
VERSION=2.01 ENCRYPTED=NO |
Resent-Sender: |
|
Message-ID: |
|
X-Incognito-SN: |
472 |
Parts/Attachments: |
|
|
Technet,
A while back there was a potential material listed that could remove
encapsulant. The material is called URESOLVE PLUS from Dyanoloy. Well, I
called the company and got some more information. Not fully understanding all
the chemistry, they said it will work an epoxy with Anhydride based
activation, but not on Amine based.
So, my question to you all, what is the chemical basis of
Photoresists, FR-4, GeTek(R), and Polyimide? I'm not looking for trade
secrets, just info that should be the MSDS sheets.
Thanks very much for your help.
Glenn Pelkey
Quality/Reliability Engineer
Maxtek Components Corp.
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|