TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain
Old-Return-Path:
Date:
Fri, 27 Jun 1997 12:05:37 -0400
Precedence:
list
Resent-From:
>From willli Fri Jun 27 10:
52:28 1997
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13688
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Fri Jun 27 11:
02:06 1997
Resent-Message-ID:
<"cBdUQ.0.I0F.W6-ip"@ipc>
Subject:
From:
Jim Herard <[log in to unmask]>
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0whdJa-000BjgC; Fri, 27 Jun 97 10:52 CDT
Resent-Sender:
TechNet-request [log in to unmask]
Message-Id:
<0042900005544970000002L002*@MHS>
Parts/Attachments:
text/plain (53 lines)
We apply our white ID silk screen  Before Hasl.

Jim Herard
KBL, Product Quality Engineering
IBM Microelectronics Endicott
t/l 857-7026

---------------------- Forwarded by Jim Herard/Endicott/IBM on 06-27-97 12:01 PM
 ---------------------------

        [log in to unmask]
        06-27-97 11:56 AM
Please respond to [log in to unmask] @ internet

To: [log in to unmask] @ internet
cc:
Subject: Idents before or after HASL

What is the most common practice:

Silkscreen idents before or after HASL?

I would appreciate any comments on this.

thanks -

Jamie McIntyre
PCI
Toronto, Canada

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2