TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wgrrk-000BjQC; Wed, 25 Jun 97 08:12 CDT
Old-Return-Path:
Date:
Wed, 25 Jun 1997 09:22:41 -0400 (EDT)
Precedence:
list
Resent-From:
Message-ID:
X-Status:
Status:
O
From [log in to unmask] Wed Jun 25 11:
19:14 1997
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"aJxvD3.0.gJE.daHip"@ipc>
Subject:
From:
>From willli Wed Jun 25 08:
12:31 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13631
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
Parts/Attachments:
text/plain (22 lines)
Ed, maybe this isn't the direction that your trying to go, but we have many
large customers that manufacture antennas.  Most of them use a hot oil reflow
process over teflon.  About a year ago Arlon ran tests different oil types.
 If your interested in information on what types of oil processes work best,
feel free to contact me.  

Scott Griggs
Applications Engineer
RBP Chemical Corp.
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2