Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wgIIp-000BjMC; Mon, 23 Jun 97 18:13 CDT |
Encoding: |
73 Text |
Old-Return-Path: |
|
Date: |
Mon, 23 Jun 97 16:29:05 cst |
From [log in to unmask] Tue Jun 24 16: |
35:17 1997 |
Resent-From: |
|
Cc: |
|
X-Status: |
|
Status: |
O |
>From willli Mon Jun 23 18: |
14:01 1997 |
TO: |
|
Return-Path: |
<TechNet-request> |
Precedence: |
list |
Resent-Message-ID: |
<"rm6WG.0.KhD.dCmhp"@ipc> |
Subject: |
|
From: |
|
X-Loop: |
|
X-Mailing-List: |
|
Resent-Sender: |
|
Message-Id: |
|
Parts/Attachments: |
|
|
Hello Rich-
ANSIJ-STD-003 is currently under revision to an "A" status with quite
a few updates, changes, etc. Please contact me offline and I'll fill
in some of info that you may be looking for.
Dave Hillman
ANSIJ-STD-003 Task Group Chairman
[log in to unmask]
319-295-1615
______________________________ Reply Separator _________________________________
Subject: Solderability Tests of Boards
Author: [log in to unmask] at ccmgw1
Date: 6/23/97 4:21 PM
Hello,
I had some difficulty with my E-mail just around the time I first
posted this. The problem is corrected , therefore here it is again.
Rich
______________________________ Forward Header __________________________________
Subject: Solderability Tests of Boards
Author: [log in to unmask] at INTERNET
Date: 6/11/97 9:04 AM
Hello,
I am interested in testing solderability of printed circuit boards.
There are 5 techniques mentioned in ANSI/J-STD-003 "Solderability
Tests for Printed Boards". They are : Edge dip, rotary dip , float,
wave, and wetting balance. The first three are done in a solder pot.
There is another method called "SERA Testing" that is not mentioned.
Do any of these prove reliable in predicting a boards performance
during assembly? Is it better to age the samples before testing? If so
then is steam aging the best method?
Interpretation of results seems to have a certain amount of
latitude. Is there a comprehensive authoritative work on the subject.
Some of the contacts for equipment manufactures mentioned in
section 6 of the document mentioned above are no longer valid. Are
there still sources for this equipment?
There is no source for wave solder testing equipment listed. Is
there a lab scale unit available?
I am interested in presenting a paper in September at the IPC
Summit on PWB Surface Finishes and Solderability in September titled
something like "Survey of Solderability Testing Techniques". I plan on
using information gathered on TECHNET in this paper. If you have
information and wish to assist please contact me.
Thanks
Rich
------------------------------------------------------------------
Richard Olsen Telephone (602)-232-9154
Continental Circuits Corp. Main (602)-268-3461
3502 East Roeser Road Fax (602)-268-0208
Phoenix Arizona Pager (602)-310-6245
85040-2905 Internet [log in to unmask]
USA I make circuit boards,what do you do?
------------------------------------------------------------------
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|