TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0weLlr-000BjtC; Wed, 18 Jun 97 09:31 CDT
Old-Return-Path:
Date:
Wed, 18 Jun 1997 10:41:33 -0400 (EDT)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/13494
TO:
Return-Path:
<TechNet-request>
>From willli Wed Jun 18 09:
32:47 1997
Resent-Message-ID:
<"52IX93.0.a6O.25_fp"@ipc>
Subject:
From:
X-Loop:
From [log in to unmask] Tue Jun 24 14:
00:42 1997
Message-ID:
Parts/Attachments:
text/plain (15 lines)
It means 5% of each land that is soldered.

Phil Hinton  

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2