Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0wX94n-000BjFC; Thu, 29 May 97 12:33 CDT |
Encoding: |
55 TEXT |
Old-Return-Path: |
<TechNet-d-request> |
Date: |
Thu, 29 May 97 11:44:00 PDT |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
X-Status: |
|
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Loop: |
|
Resent-Message-ID: |
<"2F-OP2.0.qWL.5IRZp"@ipc> |
Subject: |
|
From: |
|
From [log in to unmask] Mon Jun 2 14: |
07:16 1997 |
>From bergdi Thu May 29 12: |
33:52 1997 |
X-Mailer: |
Microsoft Mail V3.0 |
Message-Id: |
|
Parts/Attachments: |
|
|
For profiles of wavesolder temperatures, I use/ have used the following
locations
Topside PCB temp (in open area)
Bottomside PCB temp (in open area) thru a via or non plated hole
Lead of critical or heavy (ie transformer) component from topside. This
will show that the lead gets hot enough for adequate solder wicking up the
lead.
If there are concerns about a particular plated hole (one that has no
thermal relief, etc.) then we may put a thermocouple in the hole, either
with or without the component.
SMT components on the solder side may require a thermocouple at the lead or
in a hole drilled in the component, which would be filled with epoxy and
cured. This would be to test the effect of the heat on the inside of the
component.
----------
From: TechNet-request
To: technet
Subject: ASSY: MOLE temperature probes
Date: Thursday, May 29, 1997 4:46PM
Hi Technet!
A question:
To measure temperature on a PCBs you have to use a MOLE or similar with
probes (or whatever they are called).
To measure if the temperature is too high on, for example, SMDs in wave
soldering the most logic should be to put the probe on the PCB in a
SMT-components joint, right?
But where do you put the probe if you want to measure and adjust the
temperature for hole mounted components?!
We have different points of view in this matter, some say that i should
put the probes on top of the PTH and some inside the PTH.
Anyone have any suggestions?
Is there any litterature which should help?
Thanks,
Jan Merstrand
Ericsson Microwave System
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|