TECHNET Archives

June 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wcRdT-000BjMC; Fri, 13 Jun 97 03:23 CDT
Content-Type:
text/plain; charset=ISO-8859-1
Old-Return-Path:
Date:
Fri, 13 Jun 1997 04:33:03 -0400
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
MIME-Version:
1.0
From [log in to unmask] Tue Jun 17 11:
10:13 1997
X-Mailing-List:
<[log in to unmask]> archive/latest/13371
TO:
Return-Path:
<TechNet-request>
Content-Disposition:
inline
X-Status:
Status:
O
Resent-Message-ID:
<"t7bnh3.0.7eJ.hDGep"@ipc>
Subject:
From:
Karl Ring <[log in to unmask]>
X-Loop:
Message-ID:
Content-Transfer-Encoding:
quoted-printable
>From willli Fri Jun 13 03:
23:28 1997
Parts/Attachments:
text/plain (31 lines)
The measuring of ionic contamination gives some problems:

1. if there is a required limit of ionic residues check the specific
acceptance limit
   of your equipment. MIL-STD-2000A Appendix C shows a table of different
Instrument       acceptance  limits and equivalence factors.

2.Some solder masks are a good source of ionic residues. I have made
measurements of        cleaned boards with results of 13 ug/cm2. If the
solder mask is the source you can notice it     if you need a long
measuring time till the values become constant. Another method is a  
second test after baking the assembly or bare board. The result should be
lower than the first.  

3.Test the bare board. It should have max. 1.6 ug/cm2 (=3.1ug/cm2 when
using the       Ionograph).

Karl Ring
 ZVE 
Germany 
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


ATOM RSS1 RSS2