From: Scott Westheimer
Date: 6/12/97
Does anyone have specification for rinse water quality in a black oxide
line? We are trying to determine and establish quality levels for our
rinses in the horizontal black oxide line. We would also like to establish
cause and effect defects of poor rinsing. Your help would be greatly
appreciated
***************************************************************************